Estás en Construmatica.com » Materias » Ciencia de los materiales » Mecanica de fractura » Fractography: observing, measuring and interpreting fracture surface topography

Fractography: observing, measuring and interpreting fracture surface topography

Fractography: observing, measuring and interpreting fracture surface topography

12345
(Sé el primero en opinar)
Autor: Hull, Derek.
ISBN: 978-0-521-64684-0.
Editorial: Cambridge University Press
Características: 1999, 366 Págs., 1999, Inglés, Rústica.
Precio orientativo: 57,05 euros (IVA incluido).
Materia: Ciencia de los materiales.
Sub-materia: Mecanica de fractura.



Sinopsis de Fractography: observing, measuring and interpreting fracture surface topography

Fracture surfaces are produced by breaking a solid. The appearance of the surface depends on the type of material and on the conditions under which it was broken. This book covers important aspects of the study of such fracture structures. The subject has numerous applications in a wide range of materials, and is particularly relevant in materials science and to inter-disciplinary subjects involving materials science, including physics, chemistry, engineering, biomimetics, earth sciences, biology and archaeology.